Material Notes:
110 paper is a clay-filled, sheeted ceramic fiber paper which is denser and more rigid than other standard grade products. The rigidity is maintained even after burnout of the organic bonding agents. The good dielectric strength, compression resistance, and die cutting characteristics of 110 paper are advantageous in many high-temperature gasketing applications.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.288 g/cc
0.0104 lb/in³
Loss On Ignition 8.5 %
8.5 %
including binder
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.71 MPa
248 psi
As manufactured
Tensile Strength, Yield 1.01 MPa
147 psi
As manufactured
Compressive Strength 0.0276 MPa
4.00 psi
10% deformation
0.179 MPa
26.0 psi
25% deformation
1.15 MPa
167 psi
50% deformation
Thermal Properties Metric English Comments
Melting Point 1538 °C
2800 °F
Maximum Service Temperature, Air 1040 °C
1900 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 45 - 50 %
45 - 50 %
Fe2O3 <= 1.1 %
<= 1.1 %
SiO2 40 - 44 %
40 - 44 %
Descriptive Properties Value Comments
Color Tan
Na2O3 (%) <1.5
Temperature Grade (°C) 1260