Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material

Category Other Engineering Material , Composite Core Material
Manufacturer Ultracor Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ultracor® UQF-95-1/4-3.0 Honeycomb Core Material.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Construction: ±45° Quartz. Fiber: Astroquartz II. Ultracor® is a very low density honeycomb core material designed for use in highly weight-sensitive structures.  It is expected that it will be used in spacecraft Antenna Reflectors, Optical Benches, Solar Arrays, and other lightly loaded structures which must be positioned with accuracy and stability in order to properly perform their intended purpose. It was developed using a space qualified, toughened, polycyanate matrix resin. General Ultracor® features include low density, design flexibility, low CTE, low CME, and high thermal conductivity.Data provided by Ultracor Inc., formerly YLA Cellular Products Company.
Physical Properties Metric English Comments
Density 0.0480 g/cc
0.00173 lb/in³
core density
Mechanical Properties Metric English Comments
Compressive Yield Strength 1.55 MPa
225 psi
Compressive Modulus 0.172 GPa
24.9 ksi
Shear Modulus 0.117 GPa
17.0 ksi
ribbon direction
Shear Strength 1.28 MPa
186 psi
ribbon direction
Electrical Properties Metric English Comments
Dielectric Constant 1.042

@Frequency 9.50e+9 Hz
1.042

@Frequency 9.50e+9 Hz
Along ribbon
1.06

@Frequency 9.50e+9 Hz
1.06

@Frequency 9.50e+9 Hz
Across ribbon
Dissipation Factor 0.00036

@Frequency 9.50e+9 Hz
0.00036

@Frequency 9.50e+9 Hz
Across ribbon
0.00083

@Frequency 9.50e+9 Hz
0.00083

@Frequency 9.50e+9 Hz
Along ribbon