UCAR Carbon UCAR® SLX Extruded Graphite

Category Carbon , Graphite
Manufacturer UCAR Carbon Company (GrafTech International)
Trade Name UCAR®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UCAR Carbon UCAR® SLX Extruded Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Densified prior to graphitization, Grade SLX is an extruded graphite with increased densities and strength over SL.Typical Applications:CZ silicon crystal growth Quartz processing Purified electronic fixturing (after purification process) Polysilicon seed chucksTabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Particle Size <= 750 µm
<= 750 µm
Ash 0.10 %
0.10 %
Mechanical Properties Metric English Comments
Flexural Strength 24.1 MPa
3500 psi
Thermal Properties Metric English Comments
CTE, linear 3.40 µm/m-°C

@Temperature 20.0 - 100 °C
1.89 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 170 W/m-K
1180 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.000700 ohm-cm
0.000700 ohm-cm