Material Notes:
Isostatically molded ATJ has been an industry standard for many years. It is a fine grain, high strength material which can be machined to precise tolerances and a fine surface finish. Grade ATJ has unique thermal shock resistance due to the combination of low thermal expansion, high thermal conductivity and low elastic modulus.Typical Applications:Permanent molds Composite tooling Mandrels Continuous casting dies Hot pressing molds and punches Rocket motor nozzles Plungers and ramsTabular property data is typical. Information provided by UCAR Carbon Company, a GrafTech International Ltd. company.
Physical Properties Metric English Comments
Density 1.76 g/cc
0.0636 lb/in³
Particle Size 25 µm
25 µm
Ash 0.090 %
0.090 %
Mechanical Properties Metric English Comments
Flexural Strength 32.8 MPa
4750 psi
Thermal Properties Metric English Comments
CTE, linear 2.80 µm/m-°C

@Temperature 20.0 - 100 °C
1.56 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 120 W/m-K
833 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00110 ohm-cm