Material Notes:
Description: UBE Polyethylene is polymerized at high pressure using a tubular reactor. Production conditions are strictly controlled ensuring the product's superior physical and mechanical properties including transparency and glossiness, and making the material ideal for further processing.Transparency:Superior transparency and glossiness even for applications involving processing of thick objects.Ease of Processing: Excellent fluidity and melt tension characteristics suited to a wide range of molding methods.Inflation molding - can be molded into even thick or wide products with superior bubble stability.Extrusion lamination - can be drawn down even at high speed.Blow molding - can be molded producing a very smooth surface.Injection molding - can be molded even into very thin products.Strength: Good balance in length and breadth with superior tearing strength lengthways.Application: Film Features: High transparency GlossinessInformation provided by UBE.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ASTM D1505
Vinyl Acetate Content 6.0 %
6.0 %
Ube method
Melt Flow 2.0 g/10 min
2.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 96
96
ASTM D2240
Tensile Strength at Break 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 730 %
730 %
ASTM D638
Flexural Strength 10.0 MPa
1450 psi
Olsen; ASTM D747
Thermal Properties Metric English Comments
Vicat Softening Point 86.0 °C
187 °F
ASTM D1525