Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer UBE
Trade Name UBEPOL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL BR360L Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE.
Mechanical Properties Metric English Comments
Hardness, Shore A 63
63
ASTM D412
Tensile Strength at Break 19.4 MPa
2810 psi
ASTM D412
Elongation at Break 520 %
520 %
ASTM D412
100% Modulus 0.00220 GPa
0.319 ksi
ASTM D412
200% Modulus 0.00550 GPa
0.798 ksi
ASTM D412
300% Modulus 0.0102 GPa
1.48 ksi
ASTM D412
Tear Strength 48.0 kN/m
274 pli
ASTM D2240