UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=6)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer UBE
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE 7034MT2 Nylon 6/12 Monofilament (Drawing Ratio=6).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialties: Monomer containing type of 7034T, High softness Applications: Small-big size sport fishing line and long line (branch line), Softness required applicationsInformation provided by UBE.
Physical Properties Metric English Comments
Fiber Count 39200 dtex
35300 denier
Mechanical Properties Metric English Comments
Elongation at Break 40 %
40 %
Line Elongation
43 %
43 %
Knot Elongation
Tenacity 0.371 N/tex
4.20 g/denier
Knot Strength
0.547 N/tex
6.20 g/denier
Line Strength
0.794 N/tex
9.00 g/denier
Tensile Modulus
Thermal Properties Metric English Comments
Shrinkage 23 %
23 %