UBE 7034B Nylon 6/12 Copolymer Film

Category Polymer , Film , Thermoplastic , Nylon , Nylon 612 , Nylon 612, Unreinforced
Manufacturer UBE
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE 7034B Nylon 6/12 Copolymer Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Specialties: High transparencyGood thermoform-abilityLow W.V.T.R High shrink-abilityLower extrusion temperatureProcessing: Best match for co-extrusion with EVOH resins.Typical Applications: Cereal packagesFlavor barrier (compare with HDPE)Form-fill-seal (Air blown)Information provided by UBE.
Physical Properties Metric English Comments
Relative Viscosity 3.71 - 3.89 cP
3.71 - 3.89 cP
96% H2SO4
4.0 - 4.2 cP
4.0 - 4.2 cP
98% H2SO4
Thermal Properties Metric English Comments
Melting Point 195 - 205 °C
383 - 401 °F
Processing Properties Metric English Comments
Processing Temperature 190 - 200 °C
374 - 392 °F
C1
200 - 210 °C
392 - 410 °F
C2
210 - 220 °C
410 - 428 °F
C3
220 - 240 °C
428 - 464 °F
C4
230 - 250 °C
446 - 482 °F
AD
230 - 250 °C
446 - 482 °F
CF
230 - 250 °C
446 - 482 °F
D1- D4