Material Notes:
Description: T-die cast film of 25µm in thicknessInformation provided by UBE.
Physical Properties Metric English Comments
Oxygen Transmission Rate 90.0 cc/m²/day
5.80 cc/100 in²/day
0% RH,23°C
90.0 cc/m²/day
5.80 cc/100 in²/day
65% RH,23°C
180 cc/m²/day
11.6 cc/100 in²/day
100% RH,23°C
Thickness 25.0 microns
0.984 mil