Material Notes:
Specialties: Standard nylon 6/66Medium shrink, Low slipApplications: Best for Middle layer usageProcessing: Top web (Air blown)Thermoforming (T-die)Information provided by UBE.
Physical Properties Metric English Comments
Relative Viscosity 3.99 - 4.17 cP
3.99 - 4.17 cP
96% H2SO4
4.3 - 4.5 cP
4.3 - 4.5 cP
98% H2SO4
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 510 %
510 %
Film Elongation at Break, TD 560 %
560 %
Secant Modulus, MD 0.190 GPa
27.6 ksi
Secant Modulus, TD 0.200 GPa
29.0 ksi
Coefficient of Friction, Dynamic 0.51
0.51
Coefficient of Friction, Static 0.94
0.94
Film Tensile Strength at Break, MD 42.0 MPa
6090 psi
Film Tensile Strength at Break, TD 43.0 MPa
6240 psi
Thermal Properties Metric English Comments
Melting Point 191 - 201 °C
376 - 394 °F
Optical Properties Metric English Comments
Haze 11.7 %
11.7 %
Gloss 112 %
112 %
Processing Properties Metric English Comments
Processing Temperature 190 - 210 °C
374 - 410 °F
C1
220 - 230 °C
428 - 446 °F
C2
230 - 240 °C
446 - 464 °F
C3
230 - 240 °C
446 - 464 °F
C4
240 - 250 °C
464 - 482 °F
AD
240 - 250 °C
464 - 482 °F
CF
240 - 250 °C
464 - 482 °F
D1- D4
Descriptive Properties Value Comments
Degree of Curling 8 Mm