Material Notes:
Specialties: Nucleated (High viscosity) Processing: T-die, Air blownApplications: General applicationsInformation provided by UBE.
Physical Properties Metric English Comments
Relative Viscosity 3.62 - 3.8 cP
3.62 - 3.8 cP
96% H2SO4
3.88 - 4.08 cP
3.88 - 4.08 cP
98% H2SO4
Thickness 40.0 microns
1.57 mil
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 460 %
460 %
Secant Modulus, TD 0.470 GPa
68.2 ksi
Coefficient of Friction, Dynamic 0.75
0.75
20 deg. C 55% RH
Coefficient of Friction, Static 1.0
1.0
( 20 deg. C 55% RH )
Film Tensile Strength at Break, MD 98.0 MPa
14200 psi
Thermal Properties Metric English Comments
Melting Point 215 - 225 °C
419 - 437 °F
Optical Properties Metric English Comments
Haze 2.3 %
2.3 %
Gloss 145 %
145 %
Processing Properties Metric English Comments
Processing Temperature 200 - 220 °C
392 - 428 °F
C1
210 - 230 °C
410 - 446 °F
C2
230 - 240 °C
446 - 464 °F
C3
240 - 250 °C
464 - 482 °F
C4
250 - 260 °C
482 - 500 °F
AD
250 - 260 °C
482 - 500 °F
CF
250 - 260 °C
482 - 500 °F
D1- D4
Roll Temperature 80.0 °C
176 °F
Chill Roll Temperature