UBE 1024FD-1 Nylon 6 Film

Category Polymer , Film , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Film Grade
Manufacturer UBE
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE 1024FD-1 Nylon 6 Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: T-die cast film of 25µm in thicknessInformation provided by UBE.
Physical Properties Metric English Comments
Oxygen Transmission Rate 50.0 cc/m²/day
3.22 cc/100 in²/day
0% RH,23°C
54.0 cc/m²/day
3.48 cc/100 in²/day
65% RH,23°C
192 cc/m²/day
12.4 cc/100 in²/day
100% RH,23°C
Thickness 25.0 microns
0.984 mil