Material Notes:
Values and BenefitsBio-soluble fiberEasy to fabricateLow shot contentTypical ApplicationsFurance liningsThermal insulationAcoustic insulationFire protectionHeat shieldsTurbine wrapTypical Industries ServedAluminum - primary/secondaryPower GenerationApplianceFire ProtectionFoundriesPetrochemicalMarineAutomotiveCeramic IndustryInformation provided by TRITEX
Physical Properties Metric English Comments
Density 2.70 - 2.90 g/cc
0.0975 - 0.105 lb/in³
Loss On Ignition <= 0.50 %
<= 0.50 %
Filament Diameter 6.0 µm
6.0 µm
Average
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 552 MPa
80000 psi
Thermal Properties Metric English Comments
Thermal Conductivity 0.0601 W/m-K

@Temperature 260 °C
0.417 BTU-in/hr-ft²-°F

@Temperature 500 °F
0.133 W/m-K

@Temperature 538 °C
0.922 BTU-in/hr-ft²-°F

@Temperature 1000 °F
0.244 W/m-K

@Temperature 816 °C
1.69 BTU-in/hr-ft²-°F

@Temperature 1500 °F
0.327 W/m-K

@Temperature 982 °C
2.27 BTU-in/hr-ft²-°F

@Temperature 1800 °F
Melting Point >= 1100 °C
>= 2010 °F
Fiber
Maximum Service Temperature, Air 1000 °C
1830 °F
Component Elements Properties Metric English Comments
Al2O3 14 %
14 %
Primary Fiber
CaO 15 %
15 %
Primary Fiber
FeO 0.10 %
0.10 %
Primary Fiber
MgO 7.5 %
7.5 %
Primary Fiber
MnO 10 %
10 %
Primary Fiber
Other 3.4 %
3.4 %
Primary Fiber
SiO2 42 %
42 %
Primary Fiber
Descriptive Properties Value Comments
Average Fiber Length (mm) 4-8
Color off-white
Moisture Resistant Yes
Surface Treatment None
Users viewing this material also viewed the following: