Trelleborg Emerson & Cuming Stycast® E 1400 Two-Component General Purpose Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® E 1400 Two-Component General Purpose Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Typical Applications: Designed as general purpose encapsulants, these products offer a wide range of features including thermal conductivity, mechanical shock and impact resistance, as well as thermal shock protection.Emerson & Cuming E 1400 Stycast® Two-Component General Purpose EncapsulantGood Chemical ResistanceFilledThermally conductiveMix Ratio by Weight = 100:100 Cure Type: Room Temp or Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.68 g/cc
0.0607 lb/in³
Viscosity 15000 cP

@Temperature 25.0 °C
15000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
Thermal Properties Metric English Comments
CTE, linear 149 µm/m-°C

@Temperature 20.0 °C
82.8 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.740 W/m-K
5.14 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Glass Transition Temp, Tg 11.0 °C
51.8 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
Dielectric Strength 15.7 kV/mm
400 kV/in
Processing Properties Metric English Comments
Cure Time 120 - 240 min
2.00 - 4.00 hour