Trelleborg Emerson & Cuming Stycast® 4640-25 Two-Component Silicone Flexible Encapsulant

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 4640-25 Two-Component Silicone Flexible Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 4640-25 Stycast® Two-Component Silicone Flexible EncapsulantDescriptionAn RTV condensation cure. Pourable and room temperature curable.FeaturesHigh TemperaturePoor Chemical ResistanceFilledMix Ratio (by weight) = 100:0.4 Cure Type: Room Temp or Heat Bonding Type: Silicone
Physical Properties Metric English Comments
Density 0.750 g/cc
0.0271 lb/in³
Viscosity 45000 cP

@Temperature 25.0 °C
45000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 70
70
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 2.0

@Frequency 1e+6 Hz
2.0

@Frequency 1e+6 Hz
Dielectric Strength 9.84 kV/mm
250 kV/in
Processing Properties Metric English Comments
Cure Time 240 - 360 min
4.00 - 6.00 hour