Trelleborg Emerson & Cuming Stycast® 2741-15 Two-Component Epoxy Flexible Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 2741-15 Two-Component Epoxy Flexible Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 2741-15 Stycast® Two-Component Epoxy Flexible EncapsulantDescriptionElectronic embedment and sealing of metals, ceramics, and plastics. Protection of stress sensitive components where shock and impact resistance are required. Typical applications include transformers, motors, coils, and other electrical devices.FeaturesGood Chemical ResistanceFilledMix Ratio (by weight) = 100:150 Cure Type: Room Temp or Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
Viscosity 36000 cP

@Temperature 25.0 °C
36000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Thermal Properties Metric English Comments
Thermal Conductivity 0.350 W/m-K
2.43 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 65.0 °C
149 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Glass Transition Temp, Tg 11.0 °C
51.8 °F
Electrical Properties Metric English Comments
Dielectric Constant 3.3

@Frequency 1e+6 Hz
3.3

@Frequency 1e+6 Hz
Dielectric Strength 13.8 kV/mm
350 kV/in
Processing Properties Metric English Comments
Cure Time 120 - 240 min
2.00 - 4.00 hour