Trelleborg Emerson & Cuming Stycast® 2651-40FR/9 Two-Component Epoxy Flame Retardant Encapsulant

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Encapsulant, Unreinforced , Epoxy, Thermally Conductive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Stycast®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Stycast® 2651-40FR/9 Two-Component Epoxy Flame Retardant Encapsulant.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Typical ApplicationsProvide flame resistance down to 1/8 of an inch. These products also offer various other features such as thermal shock protection, low viscosity, and thermal conductivity. Typical applications include a wide range of electrical components such as capacitors and transformers.Emerson & Cuming 2651-40FR/9 Stycast® Two-Component Epoxy Flame Retardant EncapsulantThermally ConductiveGood Chemical ResistanceFilledMix Ratio by Weight = 100:9 Cure Type: Room Temp or Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
Viscosity 8000 cP
8000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Thermal Properties Metric English Comments
Thermal Conductivity 0.550 W/m-K
3.82 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 56.0 °C
133 °F
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 1e+6 Hz
3.8

@Frequency 1e+6 Hz
Dielectric Strength 17.7 kV/mm
450 kV/in
Processing Properties Metric English Comments
Cure Time 30.0 - 60.0 min
0.500 - 1.00 hour