Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features and Typical ApplicationsPrimarily designed for ease of use in either meter mix or manual dispense operations. These products also offer a wide range of features including heat dissipation, thermal and mechanical shock resistance, and thermal conductivity.Emerson & Cuming 2072 Stycast® Two-Component Easy Mix Ratio EncapsulantMix Ratio by weight = 100:50Good Chemical ResistanceLow Viscosity Cure Type: Room Temp or Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.60 g/cc
0.0578 lb/in³
Viscosity 8000 cP

@Temperature 25.0 °C
8000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 89
89
Thermal Properties Metric English Comments
CTE, linear 61.0 µm/m-°C

@Temperature 20.0 °C
33.9 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.420 W/m-K
2.91 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.2

@Frequency 1e+6 Hz
4.2

@Frequency 1e+6 Hz
Dielectric Strength 15.7 kV/mm
400 kV/in
Processing Properties Metric English Comments
Cure Time 120 - 240 min
2.00 - 4.00 hour