Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg Emerson & Cuming Eccobond® 927-10 E Needle Bonding Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 927-10 E Needle Bonding Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 927-10 E Eccobond® Needle Bonding Epoxy AdhesiveOne component, fast curing, epoxy adhesive for needle bonding with polypropylene hubs. Also recommended for bonding sealing or insulating of heat sensitive parts. Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
Viscosity 11000 cP

@Temperature 25.0 °C
11000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Adhesive Bond Strength 9.65 MPa
1400 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
18.0 min

@Temperature 90.0 °C
0.300 hour

@Temperature 194 °F
Descriptive Properties Value Comments
Color Yellow
Users viewing this material also viewed the following: