Trelleborg Emerson & Cuming Eccobond® 91 Two-Component High Strength-Peel Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 91 Two-Component High Strength-Peel Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 91 Eccobond® Two-Component High Strength-Peel Epoxy AdhesiveFiberglass filled, medium viscosity, epoxy adhesive with excellent thermal cycling properties. Used with a variety of catalysts. Designed for bonding metals exposed to high stress conditions and for bonding crystals to metals in continuous vibration applications. Mix ratio varies with amount of catalyst used. Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 1.57 g/cc
0.0567 lb/in³
Viscosity 98000 cP

@Temperature 25.0 °C
98000 cP

@Temperature 77.0 °F
Mixed
Mechanical Properties Metric English Comments
Adhesive Bond Strength 24.1 MPa
3500 psi
Descriptive Properties Value Comments
Color Black