Trelleborg Emerson & Cuming Eccobond® 56C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive , Epoxy, Electrically Conductive
Manufacturer Trelleborg Emerson & Cuming, Inc.
Trade Name Eccobond®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg Emerson & Cuming Eccobond® 56C Two-Component Silver Filled Electrically Conductive Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Emerson & Cuming 56C Eccobond® Two-Component Silver Filled Electrically Conductive Epoxy AdhesiveSilver filled, high electrical conductivity, epoxy adhesive. Excellent thermal conductivity. Requires heat cure to obtain optimal properties. Recommended for applications where hot soldering is impractical. Listed on many government specifications. Mix ratio of 100:2.5. Cure Type: Heat Bonding Type: Epoxy
Physical Properties Metric English Comments
Density 3.50 g/cc
0.126 lb/in³
Mechanical Properties Metric English Comments
Adhesive Bond Strength 5.52 MPa
800 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.00020 ohm-cm
0.00020 ohm-cm
Processing Properties Metric English Comments
Cure Time 30.0 min

@Temperature 100 °C
0.500 hour

@Temperature 212 °F
60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
Descriptive Properties Value Comments
Color Silver
Viscosity Thixotropic (Mixed, 25°C)