Material Notes:
Emerson & Cuming 23 LV Eccobond® General Purpose CatalystExcellent low temperature performance properties, excellent thermal shock/cycle and impact resistance. Good hardener for cryogenic applications. Excellent adhesion to glass. Very low viscosity, low exotherm. Light color good for clear castings. Cure Type: Room Temp or Heat
Physical Properties Metric English Comments
Density 1.01 g/cc
0.0365 lb/in³
Viscosity 20 - 30 cP

@Temperature 25.0 °C
20 - 30 cP

@Temperature 77.0 °F
Mixed
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -65.0 °C
-85.0 °F
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 65.0 °C
2.00 - 4.00 hour

@Temperature 149 °F
960 - 1440 min

@Temperature 25.0 °C
16.0 - 24.0 hour

@Temperature 77.0 °F
Pot Life 60.0 min

@Temperature 25.0 °C
60.0 min

@Temperature 77.0 °F
100 grams
Descriptive Properties Value Comments
Color Clear