Material Notes:
Emerson & Cuming 17 M 1 Eccobond® Heat Cure CatalystVery high temperature resistance, highest temperature strength, lowest shrink. Non-crystallizing. Long working life. Imparts excellent chemical resistance to cured castings. Recommended for applications requiring the optimum in high temperature performance. Cure Type: Heat
Physical Properties Metric English Comments
Density 1.40 g/cc
0.0506 lb/in³
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 230 °C
446 °F
Minimum Service Temperature, Air -20.0 °C
-4.00 °F
Processing Properties Metric English Comments
Cure Time 180 min

@Temperature 125 °C
3.00 hour

@Temperature 257 °F
Pot Life >= 1440 min

@Temperature 25.0 °C
>= 1440 min

@Temperature 77.0 °F
100 grams
Descriptive Properties Value Comments
Color Tan
Viscosity Slurry at 25°C