Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy, Electrically Conductive , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Duct
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-DUCT 916H01 is an electronically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical properties. This material was developed to be a medium to low viscosity, self leveling conductive adhesive. This two-part formulation of refined pure silver and epoxy is free of solvents and copper or carbon additives. It develops strong, durable, electrically and thermally conducting bonds and coatings between many different and dissimilar materials such as metals, ceramics, glass and plastic laminates. TRA-DUCT 916H01 cures at room temperature and can be used as a cold solder for heat-sensitive components where hot-soldering is impractical. It also can be used for the assembly and repair of electrical modules, printed circuits, wave guides, flat cables and high frequency shields. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 9500 cP

@Temperature 25.0 °C
9500 cP

@Temperature 77.0 °F
Mixed (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
1 hr @ 65°C
Adhesive Bond Strength 17.9 MPa
2600 psi
Lap shear, alum to alum, 1 hr @ 65°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 60.0 °C
140 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 0.0088 ohm-cm
0.0088 ohm-cm
cured 1 hr @ 65°C
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
Descriptive Properties Value Comments
Color Amber
Hardener
Silver
Resin/Mixed/Cured
Thixotropic Index 2
1 rpm/10 rpm