Tra-Con Tra-Coat OPL6E Low Viscosity Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Coat
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Coat OPL6E Low Viscosity Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 350 cP
350 cP
Mixed (SSA #15/7R, 100 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 45.0 °C
113 °F
Ultimate Tg
Descriptive Properties Value Comments
Color Hazy
Adhesive
Light Yellow
Cured