Material Notes:
TRA-BOND K5NA is a three-part, ablative and thermally insulating epoxy compound used in aerospace applications. This smooth, trowellable system is specified by NASA for the Space Shuttle`s solid rocket boosters for close-out and patching of the boosters` thermal protection systems. It is also used for void filling and protecting wires, tubing and other surface protrusions on hypersonic re-entry bodies, nose cones and aircraft engines. TRA-BOND K5NA is impact resistant which makes it an excellent choice for lightweight casting requirements. TRA-BOND K5NA develops strong bonds to most all substrates. It maintains excellent dimensional stability over a wide temperature range and provides protection to weathering, ozone and moisture. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 0.600 g/cc
0.600 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Mechanical Properties Metric English Comments
Hardness, Shore D 15
15
Tensile Strength, Yield 0.689 MPa
100 psi
Izod Impact, Notched 53.4 J/cm
100 ft-lb/in
Thermal Properties Metric English Comments
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 65.0 °C
2.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Light Brown
Heat of Combustion BTU/lbm 1450
Mix Ratio, parts by weight 100/75/25
Resin/Hardener/Part C
Thermal Diffusivity ft2/hr 0.0031