Tra-Con Tra-Bond FS420 Flexible Plastic Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FS420 Flexible Plastic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND FS-420 is a flexible thixotropic bonding adhesive designed for bonding all types of plastics including nylon, PVC, polyethylene, acrylic, lexan, polypropylene, kapton or almost any thermoplastic substrate. TRA-BOND FS-420 is medium viscosity and easy to apply. It has an easy 1:1 mix ratio and can be cured at room temperature. This high technology system was formulated for applications in the automotive, medical, aerospace, photonic and assemblies industries and can be used anywhere that requires excellent chemical fastening to plastic parts. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Mixed
Solids Content 97 %
97 %
Reactive Solids Content
Viscosity 22000 cP

@Temperature 25.0 °C
22000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Adhesive Bond Strength 17.2 MPa
2500 psi
Lap shear, pvc to pvc
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 115 °C
239 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 120 min
120 min
Descriptive Properties Value Comments
Color Amber
Mix Ratio, parts by weight 100/100
Resin/Hardener
Thixotropic Index 4.5
5 rpm/50 rpm