Tra-Con Tra-Bond FS25

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FS25.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 26000 cP

@Temperature 25.0 °C
26000 cP

@Temperature 77.0 °F
Mixed (rv #7, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
2 hrs @ 65°C
Adhesive Bond Strength 22.8 MPa
3300 psi
Lap shear, alum to alum, 2 hrs @ 65°C
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
Descriptive Properties Value Comments
Color Amber
Hardener/Mixed/Cured
Milky
Resin
Thixotropic Index 1.7
10 rpm/100 rpm