Tra-Con Tra-Bond FDA2YL02 Food and Drug Application Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FDA2YL02 Food and Drug Application Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND FDA-2 YL02 is a medium viscosity epoxy resin system specifically developed for adhesive and coating applications in accordance with Title 21, U.S. Code of Federal Regulations, Food and Drug Administration (FDA) Chapter 1, Sub Part B, Sections 175.105 and 175.300. This two-part opaque yellow adhesive is easily mixed and cured at room temperature. It is used for bonding, laminating and repairing food preparation, processing, packaging equipment, and biomedical applications such as catheters, hearing aids, dental products and other instruments and devices. TRA-BOND FDA-2 YL02 is an effective electrical insulator, and it provides low permeability to gases and vapors, and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants, and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 10000 cP

@Temperature 25.0 °C
10000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Elongation at Yield 9.0 %
9.0 %
Adhesive Bond Strength 12.4 MPa
1800 psi
Lap shear, alum to alum
Thermal Properties Metric English Comments
CTE, linear 53.0 µm/m-°C

@Temperature 20.0 °C
29.4 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 145 °C
293 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 54.0 °C
129 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+14 ohm-cm
1.20e+14 ohm-cm
Dielectric Constant 3.4

@Frequency 1000 Hz
3.4

@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm
420 kV/in
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
Descriptive Properties Value Comments
Color Yellow
Mix Ratio, parts by weight 100/100
Resin/Hardener
Thixotropic Index 1
5 rpm/50 rpm
Working Life hours 6.5