Tra-Con Tra-Bond F156 Optically Opaque Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond F156 Optically Opaque Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND F156 is a black, solvent-free thixotropic epoxy system recommended for high quality photographic industry bonding, laminating, production and repair applications where a room-temperature cure optically opaque adhesive for light sensitive components is required. This two-part smooth paste formulation is easy to use, develops strong bonds to itself and to most materials (including glass and glass fabrics, ceramics, leather, metals and many plastics), exhibits low shrinkage during cure, and has excellent dimensional stability over a wide temperature range. Fully cured TRA-BOND F156 has good low-temperature structural, physical and electrical properties, and is resistant to water, weather, gases, salts, mild acids and alkalis, and many organic and inorganic compounds.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 50000 cP

@Temperature 25.0 °C
50000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Thermal Properties Metric English Comments
CTE, linear 33.0 µm/m-°C

@Temperature 20.0 °C
18.3 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 130 °C
266 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.3

@Frequency 1000 Hz
4.3

@Frequency 1000 Hz
Dielectric Strength 15.4 kV/mm
390 kV/in
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Black, Opaque
Mix Ratio, parts by weight 100/12
Resin/Hardener