Tra-Con Tra-Bond CA20 Coil-Fix Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy , Filled/Reinforced Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond CA20 Coil-Fix Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND CA-20 is a thixotropic epoxy adhesive system specially formulated for shorted turns, damaged end wire extensions, or other coil repair applications where a high-fill, non-sag adhesive is required. It is dark-red to brown in color to blend with many commonly used insulating varnishes, and it provides a combination of high dielectric isolation coupled with good mechanical strength. Solvent-free TRA-BOND CA-20 is readily mixed, handled, used and cured at room temperature and develops strong bonds to most materials, including metals, glass, ceramics, and many other coil coatings and insulators. When fully cured, this epoxy adhesive provides excellent resistance to galvanic action, petroleum lubricants and solvents, salts, mild acids and alkalis, other organic and inorganic compounds, and weather.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.24 g/cc
1.24 g/cc
Mixed
Viscosity 27000 cP

@Temperature 25.0 °C
27000 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 115 °C
239 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+13 ohm-cm
6.00e+13 ohm-cm
1.00e+10 ohm-cm

@Temperature 100 °C
1.00e+10 ohm-cm

@Temperature 212 °F
Dielectric Constant 4.2

@Frequency 1000 Hz
4.2

@Frequency 1000 Hz
Dielectric Strength 15.7 kV/mm
400 kV/in
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Color Dark Red
Mix Ratio, parts by weight 100/22
Resin/Hardener