Material Notes:
TRA-BOND 970-3 general purpose adhesive is a non-flowing blue paste. This adhesive cures at room temperature. This adhesive is available in kits with a mix ratio of 100 parts A to 74 parts B or premixed and frozen in convenient, disposable syringes. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 61000 cP
61000 cP
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Adhesive Bond Strength 34.5 MPa
5000 psi
Lap shear, alum to alum
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 70.0 °C
2.00 hour

@Temperature 158 °F
2880 min

@Temperature 25.0 °C
48.0 hour

@Temperature 77.0 °F
Shelf Life 12.0 Month
12.0 Month
In kits @ 25°C
6.00 Month

@Temperature -40.0 °C
6.00 Month

@Temperature -40.0 °F
PMF
Descriptive Properties Value Comments
Color Blue
Working Life hours 1.5