Tra-Con Tra-Bond 9426M Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 9426M Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 9426M is an epoxy adhesive formulated to provide tough resilient bonds and excellent adhesion to a wide variety of substrates including metals, glass, ceramics, wood and many plastics. Information provided by Tra-Con Inc.
Mechanical Properties Metric English Comments
Hardness, Shore D 86
86
Adhesive Bond Strength 18.6 MPa
2700 psi
Lap shear, alum to alum
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 75.0 °C
2.00 hour

@Temperature 167 °F
Descriptive Properties Value Comments
Color Red