Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tra-Con Tra-Bond 9059D Rigid Unfilled Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 9059D Rigid Unfilled Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 9059D rigid, unfilled epoxy adhesive exhibits good dimensional stability for gyro applications. This material is a blue-green color.Information provided by Tra-Con Inc.
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
Adhesive Bond Strength 13.8 MPa
2000 psi
Lap shear, alum to alum, @ 25°C
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C
50.0 µin/in-°F
Above Tg
340 µm/m-°C
189 µin/in-°F
Below Tg
Glass Transition Temp, Tg 80.0 °C
176 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 100 °C
2.00 hour

@Temperature 212 °F
Shelf Life 12.0 Month

@Temperature -40.0 °C
12.0 Month

@Temperature -40.0 °F
Descriptive Properties Value Comments
Color Blue-Green
Weight Loss % 0.9
At 300°C
Working Life hours 1
Copyright © lookpolymers.com All Rights Reserved