Tra-Con Tra-Bond 862-7 General Purpose Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 862-7 General Purpose Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 862-7 semi-flexible, nonflowing epoxy paste adhesive is designed for general purpose applications. It is suitable for bonding materials with mismatched coefficients of expansion. This epoxy also offers excellent insulation. This general purpose adhesive is excellent for bonding rubber, metal, and most plastics, especially nylon. Information provided by Tra-Con Inc.
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Adhesive Bond Strength 17.2 MPa
2500 psi
Lap shear, alum to alum, @ 25°C
Thermal Properties Metric English Comments
Thermal Conductivity 0.398 W/m-K
2.76 BTU-in/hr-ft²-°F
Glass Transition Temp, Tg 40.0 °C
104 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 1.90e+12 ohm-cm

@Temperature 100 °C
1.90e+12 ohm-cm

@Temperature 212 °F
Dielectric Constant 5.5

@Frequency 1000 Hz
5.5

@Frequency 1000 Hz
Dielectric Strength 19.7 kV/mm
500 kV/in
Dissipation Factor 0.14

@Frequency 1000 Hz
0.14

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 95.0 °C
1.00 hour

@Temperature 203 °F
120 min

@Temperature 65.0 °C
2.00 hour

@Temperature 149 °F
4320 min

@Temperature 25.0 °C
72.0 hour

@Temperature 77.0 °F
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color Black
Working Life hours 1