Tra-Con Tra-Bond 723C01 One-Part Medical Grade Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 723C01 One-Part Medical Grade Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 723C01 is a fast, heat curing, one component adhesive targeted at medical applications. The material complies with USP Class VI toxicity requirements and is resistant to gamma sterilization. It is also recommended for bonding, sealing or insulating of heat sensitive parts. TRA-BOND 723C01 is often used for needle bonding applications. The adhesive adheres well to a variety of substrates including stainless steel, glass and various plastics. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
Mixed
Viscosity 16500 cP

@Temperature 25.0 °C
16500 cP

@Temperature 77.0 °F
Mixed (lv #4, 12 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
15 min @ 100°C
Adhesive Bond Strength 7.58 MPa
1100 psi
Lap shear, alum to alum, 15 min @ 100°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Glass Transition Temp, Tg 72.0 °C
162 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+14 ohm-cm
6.00e+14 ohm-cm
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 120 °C
0.167 hour

@Temperature 248 °F
15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
20.0 min

@Temperature 90.0 °C
0.333 hour

@Temperature 194 °F
Descriptive Properties Value Comments
Color Light Yellow
Thixotropic Index 1.4
3 rpm/30 rpm