Tra-Con Tra-Bond 716K02 Thixotropic Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 716K02 Thixotropic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
716K02 is a more thixotropic version of FDA2T. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 35000 cP
35000 cP
Mixed (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 82
82
1 hr @ 65°C
Adhesive Bond Strength 16.5 MPa
2400 psi
Lap shear, alum to alum, 1 hr @ 65°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 68.0 °C
154 °F
Ultimate Tg; DSC
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Descriptive Properties Value Comments
Color Amber
Hardener/Mixed/Cured
White
Resin
Thixotropic Index 3
1 rpm/10 rpm