Tra-Con Tra-Bond 716K01 Radio Opaque Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 716K01 Radio Opaque Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 716K01 is a low viscosity epoxy resin system specifically developed for adhesive coating applications where radio opacity is required. This two part dark grey adhesive is commonly used for bonding, laminating and repair applications by manufactures of catheters, guide wires, stents, processing and packaging equipment, hearing aids, dental products and other biomedical instruments and devices. TRA-BOND 716K01 provides low permeability to gases and vapors and good resistance to water, weather, galvanic action, to petroleum solvents, lubricants, and fuels, to mild acids and alkalis, and to many other organic and inorganic compounds. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 13000 cP

@Temperature 25.0 °C
13000 cP

@Temperature 77.0 °F
Mixed (cp #52, 10 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 91
91
1 hr @ 65°C
Adhesive Bond Strength 24.1 MPa
3500 psi
Lap shear, alum to alum, 1 hr @ 65°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 87.0 °C
189 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
Descriptive Properties Value Comments
Color Amber
Hardener
Dark Gray
Resin/Mixed/Cured
Thixotropic Index 1.3
1 rpm/10 rpm