Tra-Con Tra-Bond 575T01 Anaerobic Adhesive

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 575T01 Anaerobic Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 575T01 is a high strength, very fast cure, single component anaerobic retaining adhesive for fiber optic terminations. This product cures when confined in the absence of air between close fitting surfaces. A primer may be used to accelerate cure. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc
1.10 g/cc
Resin
Viscosity 1250 cP
1250 cP
Resin (rv #3, 20 rpm)
Mechanical Properties Metric English Comments
Adhesive Bond Strength 6.89 MPa
1000 psi
Lap shear, alum to alum
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 20.0 °C
44.4 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 0.100 W/m-K
0.694 BTU-in/hr-ft²-°F
Processing Properties Metric English Comments
Cure Time 0.0833 - 0.167 min
0.00139 - 0.00278 hour
Descriptive Properties Value Comments
Color Green
Resin