Tra-Con Tra-Bond 221N01

Category Polymer , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 221N01.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 3500 cP
3500 cP
Mixed (cp #52, 100 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
1 hr @ 100°C
Adhesive Bond Strength 19.3 MPa
2800 psi
Lap shear, alum to alum, 1 hr @ 100°C
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C
37.8 µin/in-°F
Below Tg
179 µm/m-°C
99.4 µin/in-°F
Above Tg
Glass Transition Temp, Tg 135 °C
275 °F
Ultimate Tg
Descriptive Properties Value Comments
Color Amber
Mixed/Cured
Brown
Hardener
Clear
Resin