Tra-Con Tra-Bond 2204

Category Polymer , Adhesive , Thermoset
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 2204.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Viscosity 60000 cP

@Temperature 25.0 °C
60000 cP

@Temperature 77.0 °F
Mixed (rv #7, 50 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
1 hr @ 65°C
Adhesive Bond Strength 10.3 MPa
1500 psi
Lap shear, alum to alum, 1 hr @ 65°C
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 32.0 °C
89.6 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 65.0 °C
1.00 hour

@Temperature 149 °F
Descriptive Properties Value Comments
Color Light Beige