Material Notes:
TRA-BOND 2135D is a medium viscosity epoxy adhesive recommended for bonding, laminating, sealing, and structural repair applications where easy mixing and good wetting combined with high impact strength properties are required. This superior, two-part adhesive is easily mixed and handled at room temperature, and develops strong, tough, high performance bonds to metals, ceramics, wood, concrete, phenolics, polyesters, epoxies, many urethanes and other plastics, and to many other materials. Fully cured TRA-BOND 2135D is a tough, durable, electrically insulating adhesive with excellent mechanical, impact and shock resistance properties. In addition, it provides good resistance to gases, vapors, weather, water, petroleum solvents, anti-icing fluids, salt solutions, many mild acids and alkalis, and many other organic materials.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 1200 cP

@Temperature 25.0 °C
1200 cP

@Temperature 77.0 °F
After mixing
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Adhesive Bond Strength 1.61 MPa
234 psi
Lap shear, alum to alum, 24 hrs @ 25°C
19.91 MPa
2888 psi
Lap shear, alum to alum, 4 hrs @ 65°C
Thermal Properties Metric English Comments
CTE, linear 55.0 µm/m-°C

@Temperature 20.0 °C
30.6 µin/in-°F

@Temperature 68.0 °F
Maximum Service Temperature, Air 100 °C
212 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 54.0 °C
129 °F
Ultimate Tg
Electrical Properties Metric English Comments
Volume Resistivity 2.70e+13 ohm-cm
2.70e+13 ohm-cm
Dielectric Constant 3.68

@Frequency 1000 Hz
3.68

@Frequency 1000 Hz
Dielectric Strength 17.1 kV/mm
435 kV/in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min
Descriptive Properties Value Comments
Color Light Amber
Mix Ratio, parts by weight 100/60
Resin/Hardener