Tra-Con Tra-Bond 1137 Epoxy Microballoon Repair Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond 1137 Epoxy Microballoon Repair Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND 1137 is a sag resistant syntactic-foam formulation developed for aerospace honeycomb, fillet, edge-fill, contour repair, bonding, potting and casting applications where a light-weight, low shrinkage and low expansion material is required. This adhesive is easily mixed and handled at room temperature, and it develops strong, highly reliable bonds to most surfaces -- including metals, glass and glass fabrics, and many plastics. TRA-BOND 1137 is a completely unicellular material composed of micron-sized phenolic spheres in a high-performance epoxy binder, has a very uniform point-to-point structure and exhibits low shrinkage during cure, good dimensional stability, low density, high strength-to-weight ratio, high dielectric strength, and a low dielectric constant. The fully cured adhesive is a strong, light weight and durable electrical insulator which can be cut, drilled sawed and shaped (as needed) with ordinary shop tools. In addition, TRA-BOND 1137 is resistant to water, weather, gases and vapors, salt and salt solutions, mild acids and alkalis, alcohol, jet fuels, gasoline and other petroleum products, and many other organic and inorganic compounds.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 0.650 g/cc
0.650 g/cc
Mixed
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 25 min
25 min
Descriptive Properties Value Comments
Color Red-Brown
Mix Ratio, parts by weight 100/18
Resin/Hardener