Material Notes:
SUPERTHERM 816H01 is a two component, thermally conductive epoxy system recommended for staking transistors, diodes, resistors, integrated circuits and other heat sensitive components to printed circuit boards. This adhesive develops strong, durable, high impact bonds at room temperature which improve heat transfer while maintaining electrical insulation. SUPERTHERM 816H01 bonds readily to itself and to metals, silica, alumina, sapphire and other ceramics, glass, plastics and many other materials, because its coefficient of thermal expansion provides a good match for those materials over a fairly wide temperature range. Fully cured SUPERTHERM 816H01 provides excellent resistance to salt solutions, mild acids and alkalais, and many other chemicals including petroleum solvents, lubricating oils, and alcohol. This adhesive complies with the requirements of NASA Outgassing Specification when tested according to ASTM E-595-90.Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Volatile Organic Compounds (VOC) Content 8.12 g/l
8.12 g/l
Viscosity 5000 cP

@Temperature 25.0 °C
5000 cP

@Temperature 77.0 °F
Mixed (rv #3)
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Adhesive Bond Strength 11.7 MPa
1700 psi
Lap shear, alum to alum
Thermal Properties Metric English Comments
CTE, linear 40.0 µm/m-°C

@Temperature 20.0 °C
22.2 µin/in-°F

@Temperature 68.0 °F
Thermal Conductivity 2.00 W/m-K
13.9 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 115 °C
239 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 54.0 °C
129 °F
Ultimate Tg
Processing Properties Metric English Comments
Cure Time 120 - 240 min

@Temperature 65.0 °C
2.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 60 min
60 min
25 grams
Descriptive Properties Value Comments
Color White
Mix Ratio, parts by weight 100/15
Resin/Hardener
Outgassing, NASA, %CVCM 0.02
3 hrs @ 65°C
Outgassing, NASA, %TWL 0.6
3 hrs @ 65°C
Working Life hours 3
25 grams