Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Toyobo ECOVYLOPET® EMC2301E PET Bottle Recycling Grade, 15% Filler Reinforced

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer Toyobo
Trade Name ECOVYLOPET®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Toyobo ECOVYLOPET® EMC2301E PET Bottle Recycling Grade, 15% Filler Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: PET Bottle Recycling Grade, 15% Filler Reinforced, Modified TypeApplications: Automobile engine head coversHot platesVending machine partsUmbrella ribsInformation provided by Toyobo.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
Water Absorption 0.050 %
0.050 %
24 hrs at 23°C
Linear Mold Shrinkage, Flow 0.012 cm/cm

@Thickness 2.00 mm
0.012 in/in

@Thickness 0.0787 in
Linear Mold Shrinkage, Transverse 0.012 cm/cm
0.012 in/in
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90
90
Tensile Strength at Break 65.0 MPa
9430 psi
Elongation at Break 3.0 %
3.0 %
Modulus of Elasticity 3.80 GPa
551 ksi
Flexural Strength 105 MPa
15200 psi
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
Thermal Properties Metric English Comments
CTE, linear 45.0 µm/m-°C

@Temperature 20.0 °C
25.0 µin/in-°F

@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 205 °C
401 °F
0.455 MPa
Processing Properties Metric English Comments
Mold Temperature 120 °C