Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Total XT10 N Natural HDPE, pipe

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Pipe Grade
Manufacturer Total Atofina
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total XT10 N Natural HDPE, pipe.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.949 g/cc
0.0343 lb/in³
ISO 1183
High Load Melt Index 7.5 g/10 min

@Load 21.6 kg
7.5 g/10 min

@Load 47.6 lb
ASTM D 1238
Mechanical Properties Metric English Comments
PENT >= 3000 hour
>= 3000 hour
ASTM F 1473
Tensile Strength, Yield >= 24.1 MPa
>= 3500 psi
ASTM D 638 type IV
Elongation at Break >= 800 %
>= 800 %
ASTM D 638 type IV
Flexural Modulus 1.03 GPa
150 ksi
ASTM D 790
Izod Impact, Notched 4.27 J/cm

@Thickness 3.17 mm
8.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Hydrostatic Design Basis 11.0 MPa

@Temperature 23.0 °C
1600 psi

@Temperature 73.4 °F
ASTM D 2837
Thermal Properties Metric English Comments
CTE, linear 180 µm/m-°C

@Temperature 20.0 °C
100 µin/in-°F

@Temperature 68.0 °F
ASTM D 696
Melting Point 131 °C
268 °F
ASTM D3417
Deflection Temperature at 0.46 MPa (66 psi) 77.8 °C
172 °F
ASTM D 648
Vicat Softening Point 124 °C
255 °F
ASTM D 1525
Brittleness Temperature -118 °C
-180 °F
ASTM D 746
Users viewing this material also viewed the following: