Total PSI 825E Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer Total Atofina
Trade Name PSI
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSI 825E Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polystyrene 825E is a high impact polystyrene designed specifically for extrusion/thermoforming. Over the years, this popular resin has established itself as the standard extrusion grade high impact polystyrene.The polymers balanced properties and processing characteristics make it especially suitable for industrial packaging deep draw thermoforming and custom multilayer sheet extrusion.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Yield 55 %
55 %
ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D638
Flexural Strength 47.6 MPa
6900 psi
ASTM D790
Flexural Modulus 2.21 GPa
320 ksi
ASTM D790
Izod Impact, Notched 1.17 J/cm
2.20 ft-lb/in
ASTM D256
Falling Dart Impact 14.11 J
10.41 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.9 °C
201 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 98.9 °C
210 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 70 %
70 %
60°; ASTM D523