Total PSC 529 Polystyrene

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Total Atofina
Trade Name PSC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total PSC 529 Polystyrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications are electronics packaging and office accessories.Information provided by Total Petrochemicals, Inc.
Physical Properties Metric English Comments
Melt Flow 3.5 g/10 min

@Load 5.00 kg,
Temperature 200 °C
3.5 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
ASTM D638
Tensile Modulus 2.96 GPa
430 ksi
ASTM D638
Flexural Strength 96.5 MPa
14000 psi
ASTM D790
Flexural Modulus 2.96 GPa
430 ksi
ASTM D790
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 92.8 °C
199 °F
Heat Distortion, Annealed; ASTM D648
Vicat Softening Point 97.8 °C
208 °F
ASTM D1525