Material Notes:
POLYSTYRENE (PS) COMPOUND (CPDS) 820 is a high impact brominated flame retardant polystyrene. A combination of high flow and high heat stability gives excellent processability and reduced cycle times. PS CPDS 820 can be supplied in both natural and colored forms.Main Characteristics:DBDPE free,Excellent UV stability,High flow, high heat stability,UL94 V2 @ 1.6 mm.Applications: Covers for electrical equipment, toner cartridges, internal enclosures for office automation.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 1.09 g/cc
1.09 g/cc
ISO 1183
Water Absorption <= 0.10 %
<= 0.10 %
ISO 62
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 200 °C
14 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ISO 1133H
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.0 MPa
2610 psi
ISO 527-2
Tensile Strength, Yield 24.0 MPa
3480 psi
ISO 527-2
Elongation at Break 45 %
45 %
ISO 527-2
Flexural Modulus 2.40 GPa
348 ksi
ISO 178
Izod Impact, Notched (ISO) 7.50 kJ/m²
3.57 ft-lb/in²
180/1A
Thermal Properties Metric English Comments
Vicat Softening Point 87.0 °C

@Load 5.10 kg
189 °F

@Load 11.2 lb
50°C per hour; ISO 306B50
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
All colors
Processing Properties Metric English Comments
Melt Temperature <= 240 °C
<= 464 °F