ATOFINA Z9450 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The very low melting point of ATOFINA Z9450 makes it an excellent heat seal layer for oriented films. Z9450 complies with FDA regulations Title 21 CFR Section 177.150 (c) 3.1 and may be used under these provisions for food contact and packaging.ApplicationATOFINA Z9450 is recommended for use in non-oriented film processes for manufacture of packaging films that require improved optical and impact properties and as a heat seal layer for oriented films. Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.890 g/cc
0.0322 lb/in³
ASTM D1505
Moisture Vapor Transmission 0.472 cc-mm/m²-24hr-atm
1.20 cc-mil/100 in²-24hr-atm
ASTM E96
Melt Flow 5.0 g/10 min
5.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 17.2 MPa
2500 psi
ASTM D882
1% Secant Modulus 345 MPa
50000 psi
ASTM D882
Dart Drop 10.6 g/micron
270 g/mil
F50; ASTM D1709
Heat Seal Strength Initiation Temperature 112 °C
234 °F
Minimum seal strength is 200 g/in at 15 psi pressure and 1 sec.; ASTM D1709
Thermal Properties Metric English Comments
Melting Point 129 °C
264 °F
DSC-2 Differential Scanning Calorimeter
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Gloss 85 %
85 %
45°; ASTM D2457
Users viewing this material also viewed the following: